Registration Dossier

Administrative data

Endpoint:
stability: thermal, sunlight, metals, other
Remarks:
Migrated from section 'Stability: thermal, sunlight, metals'
Type of information:
migrated information: read-across from supporting substance (structural analogue or surrogate)
Adequacy of study:
supporting study
Reliability:
2 (reliable with restrictions)
Rationale for reliability incl. deficiencies:
other: scientifically acceptable

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
2008
Report Date:
2008

Materials and methods

Test guideline
Qualifier:
according to
Guideline:
other: DIN 51007
Principles of method if other than guideline:
Gerätetyp: Dynamisches Wärmestromdifferenz-Kalorimeter
GLP compliance:
no

Test material

Reference
Name:
Unnamed
Type:
Constituent
Details on test material:
Name of test material (as cited in study report): Hydrocarbons, C4, 1,3-butadiene- and isobutene-free
Analytical purity: pure

Results and discussion

Any other information on results incl. tables

1. Reaktion exotherm

Onset-Temperatur 380 °C

Peak-Temperatur 451 °C

Freigesetzte Wärmemenge 60 J/g

Die Reaktion wurde nicht auf selbstbeschleunigendes Reaktionsverhalten untersucht.