Administrative data

Endpoint:
oxidising solids
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
guideline study

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Report date:
2020

Materials and methods

Test guideline
Qualifier:
according to guideline
Guideline:
EU Method A.17 (Oxidising Properties (Solids))
GLP compliance:
yes

Test material

Constituent 1
Chemical structure
Reference substance name:
Reaction mass of (24R)-ergost-5-en-3β-ol and stigmast-5-en-3-β-ol and stigmasta-5,22-dien-3-β-ol
EC Number:
904-790-6
Molecular formula:
C28H48O; C29H50O; C29H48O
IUPAC Name:
Reaction mass of (24R)-ergost-5-en-3β-ol and stigmast-5-en-3-β-ol and stigmasta-5,22-dien-3-β-ol

Results and discussion

Test results (Oxidising solids)
Sample tested:
1:1 sample-to-cellulose ratio
Parameter:
burning time of reaction over a distance of 200 mm
Result:
150 s

Any other information on results incl. tables

Mixture cellulose/test item:



































MixtureTime (s)Type of combustion
10 % test item 90 % cellulose170Ignition, orange flame
30 % test item 70 % cellulose170Ignition, orange flame
50 % test item 50 % cellulose150Ignition, orange flame
70 % test item 30 % cellulose200Ignition, orange flame
90 % test item 10% cellulose320Ignition, orange flame

Mixture cellulose/barium nitrate:










60 % reference item 40%
cellulose
300The pile burns with clear flame without
fume.

Applicant's summary and conclusion

Conclusions:
The maximum speed of combustion of barium nitrate/cellulose mixture was lower than all the test
item/cellulose mixtures, therefore the test item has oxidizing properties.