Registration Dossier

Data platform availability banner - registered substances factsheets

Please be aware that this old REACH registration data factsheet is no longer maintained; it remains frozen as of 19th May 2023.

The new ECHA CHEM database has been released by ECHA, and it now contains all REACH registration data. There are more details on the transition of ECHA's published data to ECHA CHEM here.

Diss Factsheets

Administrative data

Endpoint:
flash point of flammable liquids
Data waiving:
study technically not feasible
Justification for data waiving:
the study does not need to be conducted because the flash point is only relevant to liquids and low melting point solids
Justification for type of information:
The substance is a solid
Cross-reference
Reason / purpose for cross-reference:
data waiving: supporting information
Reference
Endpoint:
melting point/freezing point
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
test procedure in accordance with generally accepted scientific standards and described in sufficient detail
Justification for type of information:
Assessment made by manufacturer and corresponds to handbook data.
Qualifier:
equivalent or similar to guideline
Guideline:
OECD Guideline 102 (Melting point / Melting Range)
Principles of method if other than guideline:
Maplelab Scientific Melting Point Device MPD02
GLP compliance:
no
Type of method:
capillary method
Key result
Melting / freezing pt.:
> 400 °C
Decomposition:
ambiguous
Remarks:
To chromium oxide
Decomp. temp.:
> 400 °C

Experience from manufacture and use suggest that there is no specific melting point and instead the substance will oxidise at high temperatures.

Conclusions:
Experience from manufacture and use suggest that there is no specific melting point and instead the substance will oxidise at high temperatures.
Executive summary:

Substance did not melt at the upper temperature limit of the meter, 300 °C; subsequently it was placed in a furnace at a temperature >400 °C, for 2 hours. Also in this case, it was noticed that the substance still did not melt.