Registration Dossier

Administrative data

Endpoint:
relative self-ignition temperature (solids)
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
other: GLP gudeline study

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
1996
Report Date:
1996

Materials and methods

Test guideline
Qualifier:
according to
Guideline:
EU Method A.16 (Relative Self-Ignition Temperature for Solids)
GLP compliance:
yes (incl. certificate)

Test material

Reference
Name:
Unnamed
Type:
Constituent
Test material form:
solid: particulate/powder
Remarks:
migrated information: powder
Details on test material:
Name of test material (as cited in study report): 625-Triketon
Analytical purity: 99.4g/100g
Lot/batch No.: LJ 27881/1

Results and discussion

Relative self-ignition temperature (solids)
Relative self-ignition temperature:
> 400 °C
Remarks on result:
other:
Remarks:
at atm. press. of 1013.0 hPa

Any other information on results incl. tables

The test substance will no ignite itself under the test conditions.

Therefore self-heating of the substance up to 400° C is excluded

Applicant's summary and conclusion