Registration Dossier

Administrative data

Endpoint:
relative density
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
other: The density was obtained by the method described on the OECD Test Guideline according to the EU Method A.3.

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
2012
Report Date:
2012

Materials and methods

Test guideline
Qualifier:
according to
Guideline:
EU Method A.3 (Relative Density)
GLP compliance:
no
Type of method:
pycnometer method

Test material

Reference
Name:
Unnamed
Type:
Constituent
Type:
Constituent

Results and discussion

Density
Type:
relative density
Density:
ca. 1.244 g/cm³
Temp.:
20 °C

Applicant's summary and conclusion

Conclusions:
Using the picnometer method, a density of 1.2436 +-0.0003g/cm3 at 20°C+-0.2°c was measured.