Administrative data

Endpoint:
explosiveness, other
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
2 (reliable with restrictions)
Rationale for reliability incl. deficiencies:
test procedure in accordance with national standard methods with acceptable restrictions

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
1979
Report date:
1979

Materials and methods

Test guideline
Qualifier:
according to guideline
Guideline:
other: 1. sensitiveness to impact (BAM Fallhammer), 2.sensitiveness to friction (BAM friction apparatus), 3. heating under confinement (BAM)
GLP compliance:
no

Test material

Constituent 1
Chemical structure
Reference substance name:
4-(2-phenylpropan-2-yl)phenyl 4-oxo-3-(λ⁵-diazynylidene)-3,4-dihydronaphthalene-1-sulfonate
Cas Number:
23121-00-8
Molecular formula:
C25H20N2O4S
IUPAC Name:
4-(2-phenylpropan-2-yl)phenyl 4-oxo-3-(λ⁵-diazynylidene)-3,4-dihydronaphthalene-1-sulfonate
Test material form:
solid

Results and discussion

Small-scale preliminary testsopen allclose all
Parameter:
sensitiveness to impact: impact energy (J)
Remarks on result:
other: explosion (5 kg, 100 cm)
Parameter:
sensitiveness to impact: impact energy (J)
Remarks on result:
other: decompostion (5 kg, 50 cm)
Parameter:
sensitiveness to friction: friction load (N)
Remarks on result:
other: no reaction(pin load until 30 kg
Key result
Parameter:
thermal sensitivity - Koenen test: diameter of the orifice plate
Remarks on result:
other: no explosion (diameter 1.0 mm)

Any other information on results incl. tables

 

Sensitiveness to impact (BAM Fallhammer)

Weight of hammer

Height of fall

Result

5 kg

100 cm

explosion

5 kg

50 cm

decomposition

Sensitiveness to friction

Pin Load until

30 kg

no reaction

Heating under confinement (BAM)

Limiting diameter of orifice

1,0 mm

no explosion

 

The sample is not exponentially hazardous according to the law of explosives.

Applicant's summary and conclusion

Interpretation of results:
other: The sample is not exponentially hazardous according to the law of explosives.