Registration Dossier

Administrative data

Endpoint:
relative self-ignition temperature (solids)
Type of information:
experimental study
Adequacy of study:
key study
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
other: GLP guideline study

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
2012
Report Date:
2012

Materials and methods

Test guideline
Qualifier:
according to
Guideline:
EU Method A.16 (Relative Self-Ignition Temperature for Solids)
GLP compliance:
yes (incl. certificate)

Test material

Reference
Name:
Unnamed
Type:
Constituent
Test material form:
solid: crystalline

Results and discussion

Relative self-ignition temperature (solids)
Relative self-ignition temperature:
> 400 °C
Remarks on result:
other: No self-heating detected below 400 °C

Applicant's summary and conclusion