Registration Dossier

Administrative data

Endpoint:
relative self-ignition temperature (solids)
Type of information:
experimental study
Adequacy of study:
key study
Study period:
31.10.2005-01.11.2005
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
other: The study was conducted according to EU guidelines and GLP principles.

Data source

Reference
Reference Type:
study report
Title:
Unnamed
Year:
2006
Report Date:
2006

Materials and methods

Test guideline
Qualifier:
according to
Guideline:
EU Method A.16 (Relative Self-Ignition Temperature for Solids)
GLP compliance:
yes

Test material

Reference
Name:
Unnamed
Type:
Constituent

Results and discussion

Relative self-ignition temperature (solids)
Relative self-ignition temperature:
> 401 °C
Remarks on result:
other:
Remarks:
at atm. press. of 1013.0 hPa

Applicant's summary and conclusion

Conclusions:
No self-ignition of CCP-V2-1 was observed.
Executive summary:

The auto-flammability of CCP-V2 -1 was tested according to EU-method A.16. No self-ignition of CCP-V2 -1 was observed up to 401 °C.